13 August 2024 : Laboratory Research
Effects of Artificial Aging of Direct Resin Nano-Hybrid Composite on Mean Bond Strength Values for Veneer Ceramic Samples
Hafiz Adawi1ABEFG*, Kulashekar Nandalur Reddy1ABDEG, Khurshid Mattoo1ACDEG, Naif Najmi2BCEF, Majid Arishi3BCEF, Abdullah Ageeli4BCEF, Abdullah Bahri5BCEF, Shafait Ullah Khateeb6ADEG, Shan Sainudeen6ADEG, Suheel Manzoor Baba6ADEFG, Mashail M.M. Hamid7CDEG, Shahi Jahan Shah7CDEG, Sumaya Yousuf Jeri8CDEFDOI: 10.12659/MSM.945243
Med Sci Monit 2024; 30:e945243
Figure 2 Comparative distribution (number) of various failure modes observed between different types of aged direct resin composite groups (Tetric N-Ceram) and lithium disilicate ceramic (IPS e.max Press). Compiled Figure created using MS MS Word, version 20H2 (OS build 19042,1466), windows 11 Pro, Microsoft corporation).