18 January 2025 : Laboratory Research
Effect of Irrigation Solution Temperature on Bioceramic Sealer Bond Strength
Hasret KilivanDOI: 10.12659/MSM.946772
Med Sci Monit 2025; 31:e946772
Figure 3 Images of different failure types: Stereomicroscopic view of (A) cohesive bonding failure, (B) adhesive bonding failure, (C) mixed bonding failure. The photographs in Figure 3 were combined using the Paint program (Microsoft Office). No other software was used.