18 January 2025 : Laboratory Research
Effect of Irrigation Solution Temperature on Bioceramic Sealer Bond Strength
Hasret KilivanDOI: 10.12659/MSM.946772
Med Sci Monit 2025; 31:e946772
Table 3 Frequency and percentage of adhesive, cohesive, and mixed-type bonding failures by chelator group.
| GROUPS | ADHESIVE | COHESIVE | MIXED |
|---|---|---|---|
| 17% EDTA at 22°C | 1 (8.4%) | 5 (41.6%) | 6 (50%) |
| 17% EDTA at 37°C | 1 (8.4%) | 5 (41.6%) | 6 (50%) |
| 17% GA at 22°C | 2 (16.7%) | 5 (41.6%) | 5 (41.6%) |
| 17% GA at 37°C | 1 (8.4%) | 6 (50%) | 5 (41.6%) |
| 5% NaOCl at 22°C + HEDP | 3 (25%) | 6 (50%) | 3 (25%) |
| 5% NaOCl at 37°C + HEDP | 2 (16.7%) | 5 (41.6%) | 5 (41.6%) |
| EDTA – ethylenediamine tetra-acetic acid; GA – glycolic acid; NaOCl – sodium hypochlorite; Dual Rinse HEDP – etidronate powder. | |||